Hino 700 6X4 Tanker Truck 350HP 15000~16000L (For Chemical Acid Liquid, Drink Water, Oil, Carbon Steel / Stainless Steel, Lined PE Tank)
Product Description
Hino 700 6X4 Tanker Truck 350HP 15000~16000L ( For Chemical Acid Liquid ,Drink Water,Oil , Carbon Steel / Stainless Steel ,Lined PE Tank)
HINO 700 18cbm road tanker truck 350HP
15000 ~16000Litres
HINO 700Acid oil tanker truck for HCL, NaCIO acid Tank hydrochloric acid -HCL, dilute sulphuric acid WEAK SULFURIC ACID -H2SO4 ,sodium hypochlorite - NaCIO ,Caustic soda-NaOH
Customization, Cost and Control Built How You Want it, at a Price You Can Afford. for sale 86-152 -7135-7675 Steel Lined LDPE aslo for HCL(max 35%), NaOH (max 50%), NaCLO (max 10%), PAC (max 17%),H2SO4(60%,98%) ,HF ( 48%),H3PO4 (10%-85%),NH3. H2O,H2O2 (30%)
Technical specifications YC2250FS2PM5
| # | Engine model | Engine displacement | Engine power | Engine manufacturer | |||
| 1 | P11C-WB | 10520 cc | 10.5 L | 642 cuin | 240 kW | 327 hp | Shanghai Hino Engine Co., Ltd. |
| Performance | ||
| Fuel | diesel fuel | |
| Maximum speed | 80 km/h | 50 mph |
| ABS | have | |
| Weights and Ground pressure | |||
| Curb weight | 14500 kg | 14.5 | |
| Gross vehicle weight rating | 25000 kg | 25 t | 55,000 lbs |
| Axle load distribution | 7000 kg / 18000 kg (tandem axle) 7 t / 18 t (tandem axle) 15,000 lbs / 40,000 lbs (tandem axle) | ||
| Dimensions 9.42×2.5×3.97 | ||
| Overall length | 9420 mm | |
| Overall width | 2490 mm | |
| Overall height | 3970 mm | |
| Undercarriage and Suspension | ||
| Number of axles | 3 | |
| Wheelbase | 3350+1410 mm | |
| Front track | 2060 mm | 6′10″ |
| Rear track | 1855 mm / 1855 mm | 6′2″ / 6′2″ |
| Front overhang | 1460 mm | 4′10″ |
| Rear overhang | 1290 mm | 4′3″ |
| Angle of approach | 27° | |
| Angle of departure | 39° | |
| Leaf springs | 11/13,10/13 | |
| Tyres and Wheels | |
| Number of tyres | 10 |
| Tyres dimension | 11R22.5 |
| Miscellaneous | |
| Seating capacity | 2 |
| Steering control | steering wheel |
transport media name: hydrochloride, hydrogen chlorate, sodium hydroxide,
acrylic (media density are for 1190 kilograms/cubic metres),
acetic acid, glacial acetic acid, hydrogen peroxide (media density are for 1140 kilograms/cubic metres)
Propionic acid, (density for 1110 kilograms/cubic metres),
ammonia, (NH3·H2Odensity for 1090 kilograms/cubic metres),
Hydrochloric acid tank
HINO Chassis optional
Product Categories | HINO chassis | 700 chassis | |
| Product Type | FS2PMUM-TQZ | FS2PMUM-SQZ | FY2PUUM-MQZ |
| Configuration coding | W1-NR00 | W1-BL00 | W1-DL00 |
| Drive mode | 6x4 | 8x4 | |
| Maximum gross weight (kg) | 25,000 | 25,000 | 31000 |
| Cab | Standard | Standard | Standard |
| Dimensions (Length x width x height) (mm) | 8050x2495x3070 | 8050x2495x3070 | 9380x2495x3130 |
| Wheelbase (mm) | 3640 + 1410 | 3640 + 1410 | 1850 + 3400 + 1410 |
| Front / rear track (mm) | 2060/1855/1855 | 2060/1855/1855 | 2060/2060/1855/1855 |
| Front / rear overhang (mm) | 1410/1590 | 1410/1591 | 1410/1310 |
| Minimum ground clearance (mm) | ≥220 | ≥220 | ≥240 |
| Minimum turning diameter (m) | ≤18.4 | ≤18.4 | ≤20 |
| Curb weight (kg) | 9200,9400 | 9200,9400 | 11000 |
| Engine Model | P11C-VK | P11C-VK | P11C-VK |
| Rated Power (PS) kW / r / min | (350) 259/1900 | (350) 259/1900 | (350) 259/1900 |
| Maximum torque Nm / r / min | 1483/1100 | 1483/1100 | 1483/1100 |
| Post-processing system | SCR | ||
| Displacement L | 10.520 | 10.520 | 10.520 |
| Clutch | Dry-type single DSF-430 | Dry-type single DSF-430 | Dry-type single DSF-430 |
| Transmission | 12JSD160TA | RT-11509C | 12JSD160TA |
| Front / rear axle | THD17 | THD17 | THD18 |
| Rear axle Save Ratio | 4.625 | 4.625 | 5.285 |
| Tire | 11.00R20 | 11.00R20 | 11.00R20 |
| Emission standards | State IV | State IV | State IV |
Our water tank truck with different chassis, eg:DFAC, DFL, SINOTRUCK, CNHTC,NORTH BENS, FOTON, ISUZU, JAC, JMC, KAMA, YUEJIN, etc.
Rotationally Molded LLDPE TANK
chemical resistance of LLDPE Cell / :+8615271357675
www.truckinchina.com
LDPE / HDPE Chemical Resistance Chart
The chemical compatibility of LDPE and HDPE on this chart is tested at 20°C: and 50°C: for 7 days and 30 days (if applicable) with constant exposure.
| LDPE & HDPE resistance listed by chemical | |
| 1.4-dioxane | LDPE / HDPE at 20°C: little or no damage after 30 days. LDPE at 50°C: shows some effect after 7 days. |
| Acetaldehyde | LDPE / HDPE at 20°C: little or no damage after 30 days. HDPE at 50°C: shows some effect after 7 days. LDPE at 50°C: immediate damage may occur. |
| Acetic Acid 5 % | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
| Acetic Acid, glacial 50% | LDPE / HDPE at 20°C: little or no damage after 30 days. LDPE at 50 °C: immediate damage may occur. |
| Acetone | LDPE / HDPE at 20°C-50°C: damage may occur. Not recommended for continuous use. |
| Allyl Alcohol | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
| Aluminum salts | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
| Amino acids | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
| Ammonia | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
| Ammonium carbonate saturated | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
| Ammonium phosphate | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
| Ammonium sulphate | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
| Amyl chloride | HDPE at 20°C: shows some effect after 7 days. HDPE at 50°C & LDPE at 20°C-50°C: immediate damage may occur. Not recommended for continuous use. |
| Aniline | LDPE / HDPE at 20°C: little or no damage after 30 days. HDPE at 50°C: shows some effect after 7 days. |
| Benzene | LDPE / HDPE at 20°C-50°C: damage may occur. Not recommended for continuous use. |
| Benzyl alcohol | LDPE / HDPE at 50°C: immediate damage may occur. HDPE at 20°C: shows some effect after 7 days. |
| Boric acid | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
| Bromine | LDPE / HDPE at 50°C: immediate damage may occur. HDPE at 20°C: shows some effect after 7 days. |
| Butyric acid | LDPE / HDPE at 50°C: immediate damage may occur. HDPE at 20°C: shows some effect after 7 days. |
| Calcium chloride | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
| Calcium hydroxide saturated | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
| Carbon tetrachloride | HDPE at 20°C: shows little or no damage after 30 days. LDPE at 20°C & HDPE at 50°C: show some effect after 7 days. LDPE at 50°C: not recommended. |
| Chlorine 10% in water | LDPE / HDPE at 20°C: shows little or no damage after 30 days. LDPE at 50°C: shows damage and is not recommended. |
| Chlorobenzene | Immediate damage may occur. Not recommended for continuous use. |
| Chloroform | LDPE / HDPE at 20°C: show some effect after 7 days. LDPE / HDPE at 50°C: immediate damage may occur. Not recommended for continuous use. |
| Chromic acid 10% | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
| Chromic acid 50% | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
| Citric acid 10% | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
| Cresol | HDPE at 20°C: shows some effect after 7 days. LDPE at 20°C-50°C & HDPE at 50°C: show immediate damage. Not recommended for continuous use. |
| Cyclohexane | LDPE / HDPE at 50°C: immediate damage may occur. LDPE / HDPE at 20°C: show some effect after 7 days. |
| Diethyl ketone | LDPE / HDPE at 20°C-50°C: damage may occur. Not recommended for continuous use. |
| Dimethylsulfoxide | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
| Ethanol 95% | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
| Ethyl acetate | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
| Ethyl benzene | HDPE at 20°C: shows some effect after 7 days. LDPE at 20°C-50°C & HDPE at 50°C: show immediate damage. Not recommended for continuous use. |
| Ethylene glycol | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
| Ethylene oxide | HDPE at 20°C: shows little or no damage after 30 days. LDPE at 20°C: and LDPE/ HDPE at 50°C: show some effect after 7 days. |
| Ferric chloride | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
| Fluoride | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
| Fluorine | HDPE at 20°C: shows little or no damage after 30 days. LDPE at 20°C: shows some effect after 7 days. Not recommended at 50°C. |
| Formaldehyde 10% | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
| Formaldehyde 40% | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
| Glycerol | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
| Hexane | HDPE at 20°C: shows little or no damage after 30 days continuous use. HDPE at 50 °C: shows some effect after 7 days. LDPE not recommended at any temperature. |
| Hydrochloric acid 20% | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
| Hydrochloric acid 35% | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
| Hydrochloric acid 5% | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
| Hydrocyanic acid | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
| Hydrofluoric acid | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
| Hydrofluoric acid 4% | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
| Hydrofluoric acid 48% | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
| Hydrogen peroxide 3% | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
| Hydrogen peroxide 30% | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
| Isobutyl alcohol | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
| Isopropyl alcohol | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
| Kerosene | LDPE / HDPE at 20°C: show some effect after 7 days. LDPE / HDPE not recommended at 50°C, as immediate damage may occur. |
| Lactic Acid 10 % | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
| Lactic Acid 90 % | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
| Lead acetate | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
| Methanol | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
| Methyl ethyl ketone | Immediate damage may occur. Not recommended for continuous use. |
| Methyl propyl ketone | HDPE at 20°C: shows some effect after 7 days. LDPE at 20°C-50°C & HDPE at 50°C: Immediate damage may occur. Not recommended for continuous use. |
| Methylene chloride | HDPE at 20°C: shows some effect after 7 days. LDPE at 20°C-50°C & HDPE at 50°C: Immediate damage may occur. Not recommended for continuous use. |
| Mineral oil | LDPE / HDPE at 20°C: little or no damage after 30 days. LDPE at 50°C: may show immediate damage and is not recommended. |
| n-amyl acetate | LDPE / HDPE at 20°C: little or no damage after 30 days. LDPE at 50°C: shows some effect after 7 days or constant exposure. |
| n-butyl alcohol | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
| Nitric acid 50 % | LDPE at 20°C: shows little or damage after 30 days. HDPE at 20°C & LDPE at 50°C: show effect after 7 days. HDPE at 50°C: shows immediate damage and is not recommended. |
| Nitric acid 70 % | LDPE / HDPE at 20°C: show some effect after 7 days. LDPE / HDPE at 50°C: show immediate damage. Not recommended. |
| n-octane | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
| Oleic acid | HDPE at 20°C-50°C: little or no damage after 30 days. LDPE at 20°C-50°C: shows immediate damage and is not recommended. |
| Oxalic acid | LDPE at 20°C: shows some effect after 7 days. HDPE at 20°C and LDPE / HDPE at 50°C: shows little/ no damage after 30 days. |
| Ozone | LDPE / HDPE at 20°C: little or no damage after 30 days. LDPE / HDPE at 50°C: show immediate damage. Not recommended. |
| Perchloric acid | LDPE / HDPE at 20°C: little or no damage after 30 days. LDPE / HDPE at 50°C: show immediate damage. Not recommended. |
| Perchloric ethylene | LDPE / HDPE at 20°C-50°C: show immediate damage. Not recommended. |
| Phenol | LDPE / HDPE at 20°C-50°C: show immediate damage. Not recommended. |
| Phosphoric acid 10% | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
| Phosphoric acid 85% | LDPE / HDPE at 20°C: little or no damage after 30 days. LDPE at 50°C: shows immediate damage and is not recommended. |
| Phosphorous trichloride | LDPE / HDPE at 20°C: little or no damage after 30 days. LDPE at 50°C: has no data available. HDPE at 50°C: shows some effect after 7 days. |
| Potassium carbonate | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
| Potassium hydroxide 5 % | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
| Potassium hydroxide concentrated | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
| Potassium permanganate | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
| Propylene glycol | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
| Pyridine | Immediate damage may occur. Not recommended for continuous use. |
| Salicylic acid, saturated | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
| Silver acetate | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
| Silver nitrate | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
| Sodium carbonate | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
| Sodium chloride, saturated | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
| Sodium dichromate | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
| Sodium hydroxide 1% | LDPE at 20°C-50°C: shows little or no damage after 30 days. HDPE at 20°C-50°C: shows some effect after 7 days. |
| Sodium hydroxide 50% | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
| Sodium hypochlorite 15% | HDPE at 20°C-50°C: little or no damage after 30 days. LDPE at 20°C: is suitable but at 50°C: shows some effect after 7 days. |
| Sodium nitrate | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
| Sodium sulphate | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
| Sucrose | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
| Sulfuric acid 20% | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
| Sulfuric acid 6% | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
| Sulfuric acid 60% | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
| Sulfuric acid 98% | LDPE at 20°C-50°C: shows little or no damage after 30 days. HDPE at 20°C: shows effect after 7 days. Not recommended for use at 50°C. |
| Tannic acid | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
| Tetrahydrofuran | LDPE / HDPE at 20°C: show some effect after 7 day of constant exposure. LDPE / HDPE at 50°C: show immediate damage. Not recommended. |
| Toluene | LDPE at 20°C: show some effect after 7 day of constant exposure. HDPE at 20°C-50°C & LDPE at 50°C: show immediate damage. Not recommended. |
| Trichloracetic acid | LDPE / HDPE at 20°C: show some effect after 7 day of constant exposure. LDPE / HDPE at 50°C: show immediate damage. Not recommended. |
| Trichlorethane | Immediate damage may occur. Not recommended for continuous use. |
| Turpentine oil | LDPE / HDPE at 20°C: show some effect after 7 days. LDPE / HDPE at 50°C: show immediate damage. Not recommended. |
| Urea | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |
| Xylene | HDPE at 20°C: shows some effect after 7 day of constant exposure. LDPE at 20-50°C and HDPE at 50°C: show immediate damage. Not recommended. |
| Zinc chloride | LDPE / HDPE at 20°C-50°C: little or no damage after 30 days. |